钕铁硼永磁晶界扩散技术和理论发展的几个问题 |
| 刘仲武, 何家毅 |
|
Several Issues on the Development of Grain Boundary Diffusion Process for Nd-Fe-B Permanent Magnets |
| LIU Zhongwu, HE Jiayi |
| 图9 Cu的添加对烧结磁体微观组织的影响 |
| Fig.9 Effect of Cu addition on microstructure of sintered magnets (GB—grain boundary) |
|