钕铁硼永磁晶界扩散技术和理论发展的几个问题 |
| 刘仲武, 何家毅 |
|
Several Issues on the Development of Grain Boundary Diffusion Process for Nd-Fe-B Permanent Magnets |
| LIU Zhongwu, HE Jiayi |
| 图3 通过掺杂与合金化提高扩散剂速率的原理图 |
| Fig.3 Schematic of improving the diffusion efficiency via doping and alloying (The solid arrows represent the orientation of grains, and the dash arrows represent the GBD of diffusion sources) |
|