Nb-Si基超高温合金及其定向凝固工艺的研究进展 |
| 陈瑞润, 陈德志, 王琪, 王墅, 周哲丞, 丁宏升, 傅恒志 |
|
Research Progress on Nb-Si Base Ultrahigh Temperature Alloys and Directional Solidification Technology |
| CHEN Ruirun, CHEN Dezhi, WANG Qi, WANG Shu, ZHOU Zhecheng, DING Hongsheng, FU Hengzhi |
| 图3 Nbss/γ-Nb5Si3界面的HRTEM像[ |
| Fig.3 HRTEM image for Nbss/γ-Nb5Si3 interface[ |
|