埋弧焊中焊剂对焊缝金属成分调控的研究进展 |
| 王聪, 张进 |
|
Fine-Tuning Weld Metal Compositions via Flux Optimization in Submerged Arc Welding: An Overview |
| WANG Cong, ZHANG Jin |
| 图16 通过两相模型及三相模型预测的焊缝金属中Si含量与焊剂中TiO2含量的关系[ |
| Fig.16 Predicted weld metal silicon contents from slag-metal and gas-slag-metal equilibrium models as a function of TiO2 addition level in fluxes[ |
|