埋弧焊中焊剂对焊缝金属成分调控的研究进展 |
| 王聪, 张进 |
|
Fine-Tuning Weld Metal Compositions via Flux Optimization in Submerged Arc Welding: An Overview |
| WANG Cong, ZHANG Jin |
| 图13 焊缝金属中O含量与典型硅锰型焊剂中MnO含量的关系[ |
| Fig.13 Actual weld metal oxygen content as a function of MnO addition level in typical manganese-silicate type fluxes[ |
|