埋弧焊中焊剂对焊缝金属成分调控的研究进展 |
| 王聪, 张进 |
|
Fine-Tuning Weld Metal Compositions via Flux Optimization in Submerged Arc Welding: An Overview |
| WANG Cong, ZHANG Jin |
| 图10 熔渣与焊剂之间FeO含量的变化量(δFeO)与焊剂中FeO含量的关系 |
| Fig.10 Change of FeO content between slag and flux (δFeO) as a function of FeO content in FeO-SiO2(40%)-MnO fluxes |
|