埋弧焊中焊剂对焊缝金属成分调控的研究进展 |
| 王聪, 张进 |
|
Fine-Tuning Weld Metal Compositions via Flux Optimization in Submerged Arc Welding: An Overview |
| WANG Cong, ZHANG Jin |
| 图9 渣壳中FeO含量与焊缝金属中O含量的关系[ |
| Fig.9 FeO level in the slag as a function of oxygen content in the weld metal[ |
|