埋弧焊中焊剂对焊缝金属成分调控的研究进展 |
| 王聪, 张进 |
|
Fine-Tuning Weld Metal Compositions via Flux Optimization in Submerged Arc Welding: An Overview |
| WANG Cong, ZHANG Jin |
| 图7 60.00 kJ/cm线能量下ΔO与焊剂中氧化物含量的关系[ |
| Fig.7 ΔO value as a function of oxide level in fluxes under the heat input of 60.00 kJ/cm[ |
|