埋弧焊中焊剂对焊缝金属成分调控的研究进展 |
| 王聪, 张进 |
|
Fine-Tuning Weld Metal Compositions via Flux Optimization in Submerged Arc Welding: An Overview |
| WANG Cong, ZHANG Jin |
| 图6 ΔO与CaF2-SiO2-CaO焊剂中CaO含量的关系[ |
| Fig.6 ΔO value as a function of CaO content in CaF2-SiO2-CaO fluxes[ |
|