埋弧焊中焊剂对焊缝金属成分调控的研究进展 |
| 王聪, 张进 |
|
Fine-Tuning Weld Metal Compositions via Flux Optimization in Submerged Arc Welding: An Overview |
| WANG Cong, ZHANG Jin |
| 图4 量化后的O元素的过渡量(ΔO)与CaF2-SiO2焊剂中SiO2含量的关系[ |
| Fig.4 Quantified level of O transfer between flux and weld metal (WM) (ΔO) value as a function of SiO2 content in CaF2-SiO2 fluxes[ |
|