埋弧焊中焊剂对焊缝金属成分调控的研究进展 |
| 王聪, 张进 |
|
Fine-Tuning Weld Metal Compositions via Flux Optimization in Submerged Arc Welding: An Overview |
| WANG Cong, ZHANG Jin |
| 图3 不同焊接方式所对应的焊缝金属中的O、N元素的成分范围 |
| Fig.3 Expected ranges of oxygen and nitrogen contents in weld metals subjected to various welding methods (SAW—submerged arc welding, GMAW-CO2—O2 shielded metal arc welding, GMAW-Ar—Ar shielded metal arc welding, GTAW—gas tungsten arc welding, SMAW—shielded metal arc welding, SSAW—self-shielded arc welding) |
|