装甲防护陶瓷-金属叠层复合材料界面研究进展 |
| 赵宇宏, 景舰辉, 陈利文, 徐芳泓, 侯华 |
|
Current Research Status of Interface of Ceramic-Metal Laminated Composite Material for Armor Protection |
| ZHAO Yuhong, JING Jianhui, CHEN Liwen, XU Fanghong, HOU Hua |
| 图4 表面涂层技术工艺图[ |
| Fig.4 Process drawing of surface coating technology[ |
|