装甲防护陶瓷-金属叠层复合材料界面研究进展 |
| 赵宇宏, 景舰辉, 陈利文, 徐芳泓, 侯华 |
|
Current Research Status of Interface of Ceramic-Metal Laminated Composite Material for Armor Protection |
| ZHAO Yuhong, JING Jianhui, CHEN Liwen, XU Fanghong, HOU Hua |
| 图2 Ti/Al2O3叠层复合材料组织演变及裂纹扩展路径示意图[ |
| Fig.2 Schematic illustration of the microstructure evolution and crack propagation path of laminated Ti/Al2O3 composite[ |
|