装甲防护陶瓷-金属叠层复合材料界面研究进展 |
| 赵宇宏, 景舰辉, 陈利文, 徐芳泓, 侯华 |
|
Current Research Status of Interface of Ceramic-Metal Laminated Composite Material for Armor Protection |
| ZHAO Yuhong, JING Jianhui, CHEN Liwen, XU Fanghong, HOU Hua |
| 图1 由金属板支撑的陶瓷和装在金属或聚合物外壳中的陶瓷弹丸撞击的变形/破坏顺序的示意图[ (a) a ceramic tile backed by a metallic plate (b) a ceramic tile encased within a metallic or polymer case |
| Fig.1 Sketches of the deformation/failure sequence for a projectile impacting (V—velocity)[ |
|