基于增强相构型设计的石墨烯/Cu复合材料研究进展 |
| 赵乃勤, 郭斯源, 张翔, 何春年, 师春生 |
|
Progress on Graphene/Copper Composites Focusing on Reinforcement Configuration Design: A Review |
| ZHAO Naiqin, GUO Siyuan, ZHANG Xiang, HE Chunnian, SHI Chunsheng |
| 图13 三维连续石墨烯/Cu复合材料动态拉伸过程以及相应的模拟结果[ |
| Fig.13 SEM images of dynamic tensile process of three-dimensional networked Gr/Cu composites (a, b) and molecular dynamics simulation of the pull-out process of two-dimensional and three-dimensional Gr from copper matrix (c)[ |
|