基于增强相构型设计的石墨烯/Cu复合材料研究进展
|
|
赵乃勤, 郭斯源, 张翔, 何春年, 师春生
|
Progress on Graphene/Copper Composites Focusing on Reinforcement Configuration Design: A Review
|
|
ZHAO Naiqin, GUO Siyuan, ZHANG Xiang, HE Chunnian, SHI Chunsheng
|
|
图7 辅助外加工艺(累积叠轧、结构仿生法、真空抽滤)制备层状分布石墨烯/Cu复合材料示意图及微观形貌[32,33,36]
|
Fig.7 Schematic of layered distributed graphene/Cu composites prepared by cumulative rolling method (a)[32], schematic of layered distributed RGO/Cu composites prepared by biomimetic method (GrO—graphene oxide, GrO and GO have the same meaning, and GrO is only used in Fig.7; RGrO—reduced graphene oxide, RGrO and RGO have the same meaning, and RGrO is only used in Fig.7) (b)[33], SEM image of RGrO dispersed within copper matrix (c)[33], schematic of preparation of layered distributed GNPs/Cu composites by vacuum filtration (d)[36], and distributions of GNPs with different contents in copper matrix (e, f)[36]
|
|
|
|
|