超细晶铁素体-马氏体钢的高温氧化成膜特性及其对Pb-Bi腐蚀行为的影响 |
| 陈胜虎, 戎利建 |
|
Oxide Scale Formation on Ultrafine-Grained Ferritic-Martensitic Steel During Pre-Oxidation and Its Effect on the Corrosion Performance in Stagnant Liquid Pb-Bi Eutectic |
| CHEN Shenghu, RONG Lijian |
| 图8 不同变形量的冷旋锻9Cr2WVTa铁素体-马氏体钢(110)、(200)、(211)和(220)的XRD峰 |
| Fig.8 XRD peaks of (110) (a), (200) (b), (211) (c), and (220) (d) of 9Cr2WVTa ferritic-martensitic steel after cold rotary-swaging deformation rates of 0, 63%, and 94% |
|