超细晶铁素体-马氏体钢的高温氧化成膜特性及其对Pb-Bi腐蚀行为的影响 |
| 陈胜虎, 戎利建 |
|
Oxide Scale Formation on Ultrafine-Grained Ferritic-Martensitic Steel During Pre-Oxidation and Its Effect on the Corrosion Performance in Stagnant Liquid Pb-Bi Eutectic |
| CHEN Shenghu, RONG Lijian |
| 图1 9Cr2WVTa铁素体-马氏体钢经不同变形量冷旋锻变形后的微观组织 |
| Fig.1 SEM (a-c) and TEM (d-f) images of 9Cr2WVTa ferritic-martensitic steels after cold rotary-swaging deformation rates of 0 (a, d), 63% (b, e), and 94% (c, f) |
|