高强管线钢焊接临界再热粗晶区中逆转奥氏体的逆相变晶体学 |
| 李学达, 李春雨, 曹宁, 林学强, 孙建波 |
|
Crystallography of Reverted Austenite in the Intercritically Reheated Coarse-Grained Heat-Affected Zone of High Strength Pipeline Steel |
| LI Xueda, LI Chunyu, CAO Ning, LIN Xueqiang, SUN Jianbo |
| 图5 Q760、Q800和Q840试样的原位SEM像及其EBSD表征 (a1-c1) SEM images (a2-c2) band contrast maps (a3-c3) all-Euler maps |
| Fig.5 SEM images and EBSD characterizations of Q760 (a1-a3), Q800 (b1-b3), Q840 (c1-c3) samples |
|