高强管线钢焊接临界再热粗晶区中逆转奥氏体的逆相变晶体学 |
| 李学达, 李春雨, 曹宁, 林学强, 孙建波 |
|
Crystallography of Reverted Austenite in the Intercritically Reheated Coarse-Grained Heat-Affected Zone of High Strength Pipeline Steel |
| LI Xueda, LI Chunyu, CAO Ning, LIN Xueqiang, SUN Jianbo |
| 图2 X100管线钢热模拟CGHAZ组织的SEM像 |
| Fig.2 SEM images with low (a) and high (b) magnifi-cations of the simulated CGHAZ microstructure of X100 pipeline steel (CGHAZ—coarse-grained heat affected zone, M-A—martensite-austenite, GB—granular bainite, AF—acicular ferrite, LB—lath bainite) |
|