基于SH-CCT图的Q345钢焊接接头组织与硬度预测方法研究 |
| 胡龙, 王义峰, 李索, 张超华, 邓德安 |
|
Study on Computational Prediction About Microstructure and Hardness of Q345 Steel Welded Joint Based on SH-CCT Diagram |
| HU Long, WANG Yifeng, LI Suo, ZHANG Chaohua, DENG Dean |
| 图6 计算得到的铁素体和贝氏体的参数K、n |
| Fig.6 The parameters K and n of calculating ferrite and bainite, (a) and (b) got from SH-CCT1300, (c) and (d) got from SH-CCT1100, (e) and (f) got from SH-CCT900 (F—ferrite, P—pearlite, B—bainite) |
|