基于SH-CCT图的Q345钢焊接接头组织与硬度预测方法研究 |
| 胡龙, 王义峰, 李索, 张超华, 邓德安 |
|
Study on Computational Prediction About Microstructure and Hardness of Q345 Steel Welded Joint Based on SH-CCT Diagram |
| HU Long, WANG Yifeng, LI Suo, ZHANG Chaohua, DENG Dean |
| 图3 有限元模型示意图 |
| Fig.3 Schematic of finite element method (FEM) (HAZ—heat-affected zone, WM—weld metal) |
|