H13钢表面电火花沉积WC-Ni基金属陶瓷涂层微观组织及摩擦磨损性能 |
| 王文权, 杜明, 张新戈, 耿铭章 |
|
Microstructure and Tribological Properties of WC-Ni Matrix Cermet Coatings Prepared by Electrospark Deposition on H13 Steel Substrate |
| WANG Wenquan, DU Ming, ZHANG Xinge, GENG Mingzhang |
| 图6 电火花沉积WC-Ni基金属陶瓷涂层、Mo/WC-Ni复合涂层和Ni/WC-Ni复合涂层的显微硬度分布 |
| Fig.6 Microhardness distributions of WC-Ni matrix cermet coating, Mo/WC-Ni composite coating, and Ni/WC-Ni composite coating prepared by electrospark deposition |
|