高速钢表面TiN薄膜的界面疲劳剥落行为 |
| 邱龙时, 赵婧, 潘晓龙, 田丰 |
|
Interfacial Fatigue Spalling Behavior of TiN Films on High Speed Steel |
| QIU Longshi, ZHAO Jing, PAN Xiaolong, TIAN Feng |
| 图10 不同界面状态对TiN薄膜界面疲劳性能的影响 |