高速钢表面
TiN
薄膜的界面疲劳剥落行为
邱龙时, 赵婧, 潘晓龙, 田丰
Interfacial Fatigue Spalling Behavior of TiN Films on High Speed Steel
QIU Longshi, ZHAO Jing, PAN Xiaolong, TIAN Feng
图6
界面疲劳剥落机制图
Fig.6
The mechanism diagram of interfacial fatigue spalling