高速钢表面TiN薄膜的界面疲劳剥落行为 |
| 邱龙时, 赵婧, 潘晓龙, 田丰 |
|
Interfacial Fatigue Spalling Behavior of TiN Films on High Speed Steel |
| QIU Longshi, ZHAO Jing, PAN Xiaolong, TIAN Feng |
| 图3 TiN薄膜的滚动接触疲劳失效形貌的SEM像及EDS分析 (a) surface morphology (b) cross section morphology of none peeling area (c) EDS analysis |
| Fig.3 SEM images and EDS analysis of the rolling contact fatigue (RCF) failure of TiN films (t = 1.6 μm) |
|