选区激光熔化成形TiN/Inconel 718复合材料的组织和力学性能 |
||||||||||
| 王文权, 王苏煜, 陈飞, 张新戈, 徐宇欣 | ||||||||||
|
Microstructure and Mechanical Properties of TiN/Inconel 718 Composites Fabricated by Selective Laser Melting |
||||||||||
| WANG Wenquan, WANG Suyu, CHEN Fei, ZHANG Xinge, XU Yuxin | ||||||||||
| 表1 成形态IN718与不同热处理态TiN/IN718复合材料的磨损实验结果 |
||||||||||
| Table 1 Wear test results of SLMed IN718 and TiN/IN718 composites under different heat treatments |
||||||||||
|
||||||||||