微观定向结构Cu-W复合材料的力学与电学性能 |
| 韩颖, 王宏双, 曹云东, 安跃军, 谈国旗, 李述军, 刘增乾, 张哲峰 |
|
Mechanical and Electrical Properties of Cu-W Composites with Micro-Oriented Structures |
| HAN Ying, WANG Hongshuang, CAO Yundong, AN Yuejun, TAN Guoqi, LI Shujun, LIU Zengqian, ZHANG Zhefeng |
| 图8 具有微观定向结构Cu-W复合材料的有限元模型和电流密度模拟结果 |
| Fig.8 Finite element model (a) and simulated results of current density of Cu-W composites with micro-oriented W lamellas, which current flow parallel (b) and perpendicular (c) with W lamellas |
|