高应变速率多向锻造Mg-8Gd-1Er-0.5Zr合金的微观组织、织构及力学性能 |
| 丁宁, 王云峰, 刘轲, 朱训明, 李淑波, 杜文博 |
|
Microstructure, Texture, and Mechanical Properties of Mg-8Gd-1Er-0.5Zr Alloy by Multi-Directional Forging at High Strain Rate |
| DING Ning, WANG Yunfeng, LIU Ke, ZHU Xunming, LI Shubo, DU Wenbo |
| 图8 固溶态GE81K合金的孪晶面积分数和平均晶粒尺寸随累积应变的变化趋势 |
| Fig.8 Area fraction of twin and average grain size of as-solution GE81K alloy as a function of the accumulated strain |
|