高应变速率多向锻造Mg-8Gd-1Er-0.5Zr合金的微观组织、织构及力学性能 |
| 丁宁, 王云峰, 刘轲, 朱训明, 李淑波, 杜文博 |
|
Microstructure, Texture, and Mechanical Properties of Mg-8Gd-1Er-0.5Zr Alloy by Multi-Directional Forging at High Strain Rate |
| DING Ning, WANG Yunfeng, LIU Ke, ZHU Xunming, LI Shubo, DU Wenbo |
| 图4 固溶态GE81K合金在ΣΔε为1.98和2.64时的反极图和孪晶分布图 |
| Fig.4 Inverse pole figures (a, b) and twin distribution maps (c, d) of as-solution GE81K alloy at ΣΔε = 1.98 (a, c) and ΣΔε = 2.64 (b, d) (DRX—dynamic recrystallization) |
|