高应变速率多向锻造Mg-8Gd-1Er-0.5Zr合金的微观组织、织构及力学性能 |
| 丁宁, 王云峰, 刘轲, 朱训明, 李淑波, 杜文博 |
|
Microstructure, Texture, and Mechanical Properties of Mg-8Gd-1Er-0.5Zr Alloy by Multi-Directional Forging at High Strain Rate |
| DING Ning, WANG Yunfeng, LIU Ke, ZHU Xunming, LI Shubo, DU Wenbo |
| 图2 固溶态Mg-8Gd-1Er-0.5Zr (GE81K)合金的OM像及XRD谱 |
| Fig.2 OM image (a) and XRD spectrum (b) of as-solution Mg-8Gd-1Er-0.5Zr (GE81K) alloy |
|