Mn和In添加对SmCo7结构稳定性及磁矩影响的第一性原理计算 |
| 毛斐, 吕皓, 唐法威, 郭凯, 刘东, 宋晓艳 |
|
First-Principle Calculation on the Effect of Mn and In on the Structural Stability and Magnetic Moment of SmCo7 Alloys |
| MAO Fei, LU Hao, TANG Fawei, GUO Kai, LIU Dong, SONG Xiaoyan |
| 图3 4种SmCo7晶体结构模型对应的XRD模拟结果与实验结果[ |
| Fig.3 Comparison for the simulated XRD peak positions among the four SmCo7 structure models and the experimental result[ |
|