Cu含量对SiC/Al-Mg-Si-Cu复合材料自然时效负面效应的影响 |
| 朱士泽, 王东, 王全兆, 肖伯律, 马宗义 |
|
Influence of Cu Content on the Negative Effect of Natural Aging in SiC/Al-Mg-Si-Cu Composites |
| ZHU Shize, WANG Dong, WANG Quanzhao, XIAO Bolv, MA Zongyi |
| 图1 17%SiC (体积分数)/Al-1.2Mg-0.6Si-1.0Cu (质量分数,%)复合材料AA(淬火后立刻在170℃下人工时效6 h)状态下微观组织的OM及SEM像 |
| Fig.1 OM (a) and SEM (b) images of the 17% (volume fraction) SiC/Al-1.2Mg-0.6Si-1.0Cu (mass fraction, %) composites in the AA state (artificial aging at 170oC for 6 h immediately after quenching) |
|