NiTi-NbTi原位复合材料的Lüders带型变形和载荷转移行为 |
| 姜江, 郝世杰, 姜大强, 郭方敏, 任洋, 崔立山 |
|
Lüders-Like Deformation and Stress Transfer Behavior in an In Situ NiTi-NbTi Composite |
| JIANG Jiang, HAO Shijie, JIANG Daqiang, GUO Fangmin, REN Yang, CUI Lishan |
| 图4 TiNi-NbTi复合材料的均匀变形和Lüders带型变形示意图 |
| Fig.4 Schematics of homogenous deformation and Lüders-like deformation of TiNi-NbTi composite (a-e) (P—B2-NiTi parent phase, M—martensite; εi—macro strain of the composite, σ—stress) |
|