奥氏体316不锈钢中位错与氢的相互作用机理 |
| 安旭东, 朱特, 王茜茜, 宋亚敏, 刘进洋, 张鹏, 张钊宽, 万明攀, 曹兴忠 |
|
Interaction Mechanism of Dislocation and Hydrogen in Austenitic 316 Stainless Steel |
| AN Xudong, ZHU Te, WANG Qianqian, SONG Yamin, LIU Jinyang, ZHANG Peng, ZHANG Zhaokuan, WAN Mingpan, CAO Xingzhong |
| 图4 500℃退火1 h样品在不同充氢条件下的W参数和ΔW参数与正电子入射能量的关系曲线 |
| Fig.4 W-E (a) and ΔW-E (b) curves of austenitic 316 stainless steel under different hydrogen charging conditions after annealing at 500oC for 1 h (ΔW—the increment of W, ΔW4—the difference of W parameters between No.3 and No.4, ΔW5—the difference of W parameters between No.3 and No.5, ΔW6—the difference of W parameters between No.3 and No.6) |
|