模压变形中国低活化马氏体钢沉淀相对其力学性能的影响 |
| 薛克敏, 盛杰, 严思梁, 田文春, 李萍 |
|
Influence of Precipitation of China Low Activation Martensitic Steel on Its Mechanical Properties After Groove Pressing |
| XUE Kemin, SHENG Jie, YAN Siliang, TIAN Wenchun, LI Ping |
| 图6 不同道次模压变形前后CLAM钢的抗拉强度、延伸率曲线和三道次模压变形后拉伸断口形貌的SEM像 |
| Fig.6 Tensile strength and elongation curves of CLAM steel with different groove pressing passes (a) and SEM image showing the fracture merphology of tensile specimen after three-passes groove pressing (b) |
|