M-A岛高温回火转变产物对核电SA508-3钢冲击韧性影响机制 |
| 蒋中华, 杜军毅, 王培, 郑建能, 李殿中, 李依依 |
|
Mechanism of Improving the Impact Toughness of SA508-3 Steel Used for Nuclear Power by Pre-Transformation of M-A Islands |
| JIANG Zhonghua, DU Junyi, WANG Pei, ZHENG Jianneng, LI Dianzhong, LI Yiyi |
| 图7 正火态SA508-3钢试样经不同预处理后TEM像和SAED花样 |
| Fig.7 TEM images and corresponding SAED patterns (insets) of as-normalized sample of SA508-3 steel after different pre-treatments of cryogenic treatment at -196oC (a) and tempering at 200oC (b), 300oC (c), 400oC (d, e), and 450oC (f) (Fig.7e is the enlarged image of the rectangle region in Fig.7d) |
|