M-A岛高温回火转变产物对核电SA508-3钢冲击韧性影响机制 |
| 蒋中华, 杜军毅, 王培, 郑建能, 李殿中, 李依依 |
|
Mechanism of Improving the Impact Toughness of SA508-3 Steel Used for Nuclear Power by Pre-Transformation of M-A Islands |
| JIANG Zhonghua, DU Junyi, WANG Pei, ZHENG Jianneng, LI Dianzhong, LI Yiyi |
| 图4 SA508-3钢正火态显微组织 (a) EBSD image quality map showing the different phases (BF—bainitic ferrite in grey, AR in red, M in dark grey) (b) TEM bright-field image of blocky AR island and corresponding selected area electron diffraction (SAED) pattern (inset) (c) TEM bright-field image from region 1 in Fig.4b (d) TEM bright-field image of twined M island and SAED pattern (inset) |
| Fig.4 As-normalized microstructures of SA508-3 steel |
|