SEBM成形片状极小曲面点阵材料的力学性能
樊永霞, 王建, 张学哲, 王建忠, 汤慧萍

Mechanical Property of Shell Minimal Surface Lattice Material Printed by SEBM
FAN Yongxia, WANG Jian, ZHANG Xuezhe, WANG Jianzhong, TANG Huiping
图5 SEBM成形Ti-6Al-4V D型TPMS点阵材料典型压缩应力-应变曲线
Fig.5 Typical stress-strain curve of SEBM manufactured Ti-6Al-4V type D TPMS lattice material