SEBM成形片状极小曲面点阵材料的力学性能 |
| 樊永霞, 王建, 张学哲, 王建忠, 汤慧萍 |
|
Mechanical Property of Shell Minimal Surface Lattice Material Printed by SEBM |
| FAN Yongxia, WANG Jian, ZHANG Xuezhe, WANG Jianzhong, TANG Huiping |
| 图4 SEBM成形Ti-6Al-4V金刚石(D)型TPMS点阵材料显微组织的OM像 |
| Fig.4 Low (a) and high (b) magnified OM images of SEBM manufactued Ti-6Al-4V type D TPMS lattice material (The arrows show the building directions) |
|