SEBM成形片状极小曲面点阵材料的力学性能
樊永霞, 王建, 张学哲, 王建忠, 汤慧萍

Mechanical Property of Shell Minimal Surface Lattice Material Printed by SEBM
FAN Yongxia, WANG Jian, ZHANG Xuezhe, WANG Jianzhong, TANG Huiping
图3 SEBM成形Ti-6Al-4V三周期极小曲面(TPMS)点阵材料表面形貌的SEM像
(a) D (top) (b) G (top) (c) I (top) (d) P (top) (e) G (side) (f) G (bottom)
Fig.3 SEM images of the SEBM manufactured Ti-6Al-4V TPMS lattice material (For arrowed sample, the arrow shows the building direction while for the arrow-free samples, building direction is perpendicular to the image plane)