SEBM成形片状极小曲面点阵材料的力学性能 |
| 樊永霞, 王建, 张学哲, 王建忠, 汤慧萍 |
|
Mechanical Property of Shell Minimal Surface Lattice Material Printed by SEBM |
| FAN Yongxia, WANG Jian, ZHANG Xuezhe, WANG Jianzhong, TANG Huiping |
| 图2 电子束选区熔化(SEBM)成形Ti-6Al-4V点阵材料的宏观形貌 (a) O (b) T (c) D (d) G (e) I (f) P |
| Fig.2 Macrostructures of Ti-6Al-4V lattice material manufactured by selective electron beam melting (SEBM) |
|