Mg-4.4Li-2.5Zn-0.46Al-0.74Y合金高温变形流动应力、组织演变与本构分析 |
| 曹富荣, 丁鑫, 项超, 尚会会 |
|
Flow Stress, Microstructural Evolution, and Constitutive Analysis During High-Temperature Deformation in Mg-4.4Li-2.5Zn-0.46Al-0.74Y Alloy |
| CAO Furong, DING Xin, XIANG Chao, SHANG Huihui |
| 图6 lnZ-ln[sinh(ασ)]关系曲线以及计算应力与测量应力的比较 |
| Fig.6 Relation curve of lnZ-ln[sinh(ασ)] (a), and comparison of calculated stress and measured stress (b) (Z—Zener-Hollomon parameter, r2—related coefficient) |
|