Mg-4.4Li-2.5Zn-0.46Al-0.74Y合金高温变形流动应力、组织演变与本构分析
|
|
曹富荣, 丁鑫, 项超, 尚会会
|
Flow Stress, Microstructural Evolution, and Constitutive Analysis During High-Temperature Deformation in Mg-4.4Li-2.5Zn-0.46Al-0.74Y Alloy
|
|
CAO Furong, DING Xin, XIANG Chao, SHANG Huihui
|
|
图5 高温拉伸条件下LZAY4301合金的ln-lnσ、ln-σ、ln-ln[sinh(ασ)]和ln[sinh(ασ)]-1 / T关系曲线
|
Fig.5 Curves of ln-lnσ (a), ln-σ (b), ln-ln[sinh(ασ)] (c), and ln[sinh(ασ)]-1 / T (d) of LZAY4301 alloys under high temperature tensile condition (—strain rate, σ—true stress, α—stress multiplier factor, T—absolute temperature; the number adjacent to the regression line indicates specific slope)
|
|
|
|
|