Mg-4.4Li-2.5Zn-0.46Al-0.74Y合金高温变形流动应力、组织演变与本构分析 |
| 曹富荣, 丁鑫, 项超, 尚会会 |
|
Flow Stress, Microstructural Evolution, and Constitutive Analysis During High-Temperature Deformation in Mg-4.4Li-2.5Zn-0.46Al-0.74Y Alloy |
| CAO Furong, DING Xin, XIANG Chao, SHANG Huihui |
| 图3 LZAY4301合金退火态的XRD谱 |
| Fig.3 XRD spectrum of LZAY4301 alloy annealed at 523 K for 1h |
|