核聚变堆偏滤器热沉材料研究现状及展望 |
| 彭吴擎亮, 李强, 常永勤, 王万景, 陈镇, 谢春意, 王纪超, 耿祥, 黄伶明, 周海山, 罗广南 |
|
A Review on the Development of the Heat Sink of the Fusion Reactor Divertor |
| PENG Wuqingliang, LI Qiang, CHANG Yongqin, WANG Wanjing, CHEN Zhen, XIE Chunyi, WANG Jichao, GENG Xiang, HUANG Lingming, ZHOU Haishan, LUO Guangnan |
| 图7 中子辐照对CuCrZr IG和CuAl25 IG均匀延伸率的影响[ |
| Fig.7 Radiation damage dose effect on the uniform elongation of CuCrZr IG (a) and CuAl25 IG (b) alloys (CR + ann—cross-rolled and annealed at 1000oC, 1 h; SA + aged—solution annealing at 980°C, 1 h, and ageing at 480°C, 4 h)[ |
|