一种新分组团簇动力学模型模拟铝合金中的Al3Sc析出
许坤, 王海川, 孔辉, 吴朝阳, 张战

Precipitation Kinetics of Al3Sc in Aluminum Alloys Modeled with a New Grouping Cluster Dynamics Model
XU Kun, WANG Haichuan, KONG Hui, WU Zhaoyang, ZHANG Zhan
图4 300℃等温析出时归一化Al3Sc尺寸分布计算结果与实验测量和LSW分布的比较
Fig.4 Comparison of calculated and measured normalized precipitate size distributions of Al3Sc precipitates during isothermally ageing at 300oC and LSW distribution for 6 h (a), 72 h (b), and 350 h (c) (g(rˉ)=ΔN?/?NP/Δr?/?rP, r—radius, rˉ—normalize radius, ΔN—total number density of clusters in each size group, Δr—radius interval of clusters in each size group)