模拟近海大气环境下结构钢锈蚀表面特征随机模型
|
|
王友德, 周晓东, 马蕊, 徐善华
|
Stochastic Model for Surface Characterization of Structural Steel Corroded in Simulated Offshore Atmosphere
|
|
WANG Youde, ZHOU Xiaodong, MA Rui, XU Shanhua
|
|
表1 锈蚀深度与锈坑特征参数统计结果
|
Table 1 Corrosion depth parameters and pitting characteristic parameters
|
|
Sample No. | Δte μm | Δtave μm | tsd μm | a | b | Pd cm-2 | μh | σh | μAr | σAr |
|---|
| S1-1 | 114 | 58 | 24 | 1.618 | 1.062 | 15.3 | 4.55 | 0.24 | 2.21 | 0.44 | | S1-2 | 119 | 62 | 26 | 1.867 | 1.031 | 19.8 | 4.23 | 0.15 | 2.19 | 0.41 | | S2-1 | 374 | 157 | 78 | 2.369 | 1.583 | 21.9 | 5.33 | 0.19 | 1.60 | 0.50 | | S2-2 | 379 | 192 | 87 | 2.458 | 1.635 | 19.0 | 5.49 | 0.33 | 1.53 | 0.55 | | S3-1 | 552 | 212 | 101 | 2.124 | 1.374 | 18.5 | 5.64 | 0.25 | 1.33 | 0.61 | | S3-2 | 540 | 160 | 87 | 2.215 | 1.382 | 15.6 | 5.40 | 0.38 | 1.49 | 0.63 | | S4-1 | 582 | 227 | 72 | 2.271 | 1.501 | 18.0 | 5.62 | 0.22 | 1.31 | 0.62 | | S4-2 | 602 | 234 | 129 | 1.535 | 0.844 | 13.4 | 5.56 | 0.47 | 1.50 | 0.47 | | S5-1 | 692 | 261 | 121 | 3.306 | 1.955 | 23.0 | 5.60 | 0.48 | 1.56 | 0.55 | | S5-2 | 698 | 210 | 76 | 1.338 | 0.853 | 24.1 | 5.72 | 0.17 | 1.37 | 0.39 | | S6-1 | 796 | 267 | 107 | 2.644 | 1.598 | 25.1 | 5.97 | 0.26 | 1.19 | 0.55 | | S6-2 | 808 | 207 | 95 | 2.429 | 1.442 | 21.8 | 5.66 | 0.27 | 1.19 | 0.50 | | S7-1 | 1091 | 293 | 109 | 2.531 | 1.546 | 21.1 | 5.95 | 0.23 | 1.07 | 0.59 | | S7-2 | 1144 | 395 | 126 | 2.613 | 1.609 | 20.9 | 6.28 | 0.13 | 0.81 | 0.61 | | S8-1 | 1387 | 360 | 107 | 2.438 | 1.469 | 23.5 | 6.22 | 0.17 | 0.79 | 0.54 | | S8-2 | 1434 | 397 | 128 | 2.024 | 1.198 | 19.0 | 6.38 | 0.14 | 0.74 | 0.48 |
|
|
|