模拟近海大气环境下结构钢锈蚀表面特征随机模型 |
| 王友德, 周晓东, 马蕊, 徐善华 |
|
Stochastic Model for Surface Characterization of Structural Steel Corroded in Simulated Offshore Atmosphere |
| WANG Youde, ZHOU Xiaodong, MA Rui, XU Shanhua |
| 图9 锈坑深度对数均值(μh)和锈坑径深比对数均值(μAr)变化规律 |
| Fig.9 Changing laws of μh (a) and μAr (b) relative to Δtave |
|