模拟近海大气环境下结构钢锈蚀表面特征随机模型 |
| 王友德, 周晓东, 马蕊, 徐善华 |
|
Stochastic Model for Surface Characterization of Structural Steel Corroded in Simulated Offshore Atmosphere |
| WANG Youde, ZHOU Xiaodong, MA Rui, XU Shanhua |
| 图2 模拟与自然[ |
| Fig.2 Comparisons between the corrosion losses of steel under accelerated and natural[ |
|